Step 1 of 3
Understand it
The short answer, then why it happens.
The short answer
Concrete hardens by a chemical reaction between cement and water, and the reaction needs water and mild temperatures to keep going. If the surface dries out in sun or wind, or freezes in the first days, the reaction stalls and the slab ends up weaker, dustier and more prone to cracking and scaling. Curing means protecting the pour: keeping it damp or covered, shielding it from extremes and keeping traffic off it while it gains strength.
Concrete does not dry, it cures
Most people assume concrete hardens the way paint dries, by losing water.
It is the opposite. Cement reacts with water to form the bonds that hold the stone and sand together, and that reaction takes time. The more completely it happens, the stronger and denser the slab.
That is why a slab that looks and feels hard after a day is nowhere near full strength. Strength builds over weeks, and it is commonly measured at 28 days as a standard point of reference. The first few days matter most.
Step 2 of 3
See it
Each picture sits right after the section it explains.
See itIllustrates section 01: Concrete does not dry, it cures
Watch it happen
Watch concrete cure instead of dry
A slab is poured and levelled while wet, hardens to a pale grey that looks finished, then is covered with wet burlap and misted so the first days keep the water in.
1. Cement reacts with water
Cement reacts with water to form the bonds that hold the stone and sand together, and that reaction takes time.
2. Hard is not strong
That is why a slab that looks and feels hard after a day is nowhere near full strength. Strength builds over weeks, and it is commonly measured at 28 days as a standard point of reference.
3. The first few days matter most
The first few days matter most.
What happens when it dries too fast
Sun, wind and low humidity pull water out of the surface faster than the slab can bring it up from within.
The top layer then stops reacting. It ends up weak, powdery and thinly bonded, and it is also the layer that takes the wear, the salt and the freeze.
Fast drying also causes shrinkage cracks, because the surface shrinks while the concrete beneath is still stable. Fine, random cracks on a new slab, called crazing, are a common sign.
See itIllustrates section 02: What happens when it dries too fast
Watch it happen
What happens when a slab dries too fast
Sun and wind pull water off the surface, the top layer goes powdery, fine cracks appear, and then the same slab is covered with wet burlap or sealed with a curing compound.
1. Sun and wind pull water out
Sun, wind and low humidity pull water out of the surface faster than the slab can bring it up from within.
2. The top layer stops reacting
The top layer then stops reacting. It ends up weak, powdery and thinly bonded, and it is also the layer that takes the wear, the salt and the freeze.
3. Shrinkage cracks
Fast drying also causes shrinkage cracks, because the surface shrinks while the concrete beneath is still stable. Fine, random cracks on a new slab, called crazing, are a common sign.
4. Keep it damp
The slab can be kept damp by misting or covering it with wet burlap or plastic sheeting.
5. Or seal the water in
A curing compound can be sprayed on to seal moisture in. Either way the aim is the same: keep water in the surface for the first days.
Cold and hot weather
Cold slows the reaction, and a freeze in the first day or two can damage the slab for good.
Water in fresh concrete expands when it freezes and breaks up the bonds before they have formed. A slab frozen early may look fine and then scale badly later.
Good practice in cold weather is to avoid pouring when a hard freeze is coming, or to protect the pour with blankets and other insulation. A surface that is frozen when the concrete goes onto it is a bad start in any case.
Heat speeds the set and makes finishing harder. The surface can skin over while the concrete below is still soft, which traps water and leaves a weak top. In hot or windy conditions, crews pour early, wet the base, shade the work or schedule a quick start on curing.
If a contractor is pouring on a very hot, windy afternoon and has no plan for it, that is worth a question.
See itIllustrates section 03: Cold and hot weather
Watch it happen
What a freeze does to fresh concrete
A freshly poured slab freezes, ice forms inside it, the surface later scales, and a blanket over the pour is the protection.
1. A freeze in the first day or two
Cold slows the reaction, and a freeze in the first day or two can damage the slab for good.
2. Ice forms before the bonds do
Water in fresh concrete expands when it freezes and breaks up the bonds before they have formed.
3. It may look fine, then scale
A slab frozen early may look fine and then scale badly later.
4. Protect the pour
Good practice in cold weather is to avoid pouring when a hard freeze is coming, or to protect the pour with blankets and other insulation.
How curing is done
There are a few ways. The slab can be kept damp by misting or covering it with wet burlap or plastic sheeting.
A curing compound can be sprayed on to seal moisture in. Either way the aim is the same: keep water in the surface for the first days.
Do not add water to the surface while finishing. That is a different mistake, and it weakens the top layer. Water belongs in the curing, not the finishing.
What owners can do, and what to ask
Respect the wait times you are given.
Keep foot traffic off until told, and vehicles off much longer, because a young slab can be damaged by loads it would carry easily later. Keep sprinklers and downspouts from flooding or washing the surface unevenly.
Delay winter salt on a slab poured late in the year. Fresh concrete is more vulnerable to salt damage, and the first winter is the hardest one. We cover why in our guide to salt and scaling.
Ask how the slab will be cured, how it will be protected if the weather turns, and when you can walk and drive on it. A crew that has a clear answer works with the process.
If you have a slab that looks dusty or scaled after its first season, send us photos. We do concrete flatwork and repair, and we can usually tell whether curing was a factor.
Spotting a poorly cured slab
A slab that was cured badly often gives itself away in its first year.
The surface may be dusty, so that a dark shoe leaves a pale mark, or it may be rough and flaking in patches. Fine map like cracks across the surface, called crazing, are another sign, as are scaled areas after the first winter.
None of these always means a bad pour, since other things cause them too. But if several show up together on a slab that was poured in extreme weather, curing is a likely suspect.
Document the slab with photographs when it is new, and again at the end of its first winter. It makes it far easier to tell what changed and when, and it gives a clear picture to anyone you ask for help.
Step 3 of 3
Act on it
Quick answers, where to read next, and how we can help.
Questions people ask
Is it bad to pour concrete when it rains?
Light rain on a finished slab can mar the surface, and heavy rain can wash it. A crew should protect the pour or postpone it. Rain does not hurt the curing itself, since water is what concrete needs.
How long before I can park on a new slab?
Longer than most people want. Your installer will give a time for foot traffic and a longer one for vehicles. Following it protects the slab for its whole life.
Why is my new concrete dusty?
Dusting usually means the surface was weakened by early drying, extra water in the finish or a frozen start. It can sometimes be treated with a hardener or sealer.
Should I hose down a new slab?
A light misting in hot, dry weather can help keep it damp, if the installer agrees. Do not flood it or let water pool.
Does sealing help curing?
A curing and sealing compound applied right after finishing holds moisture in. A decorative sealer applied weeks later is a different product and does not do the same job.
Does curing continue after the first month?
Yes, strength keeps building slowly for months and years if there is moisture. The first week matters most, but the slab is not at full strength after a month.
Seeing this at your place?
Send us a few photos through the contact page and the chat there, and we'll tell you what we think.
Request an estimateOur masonry and concrete workAll guides