Step 1 of 3
Understand it
The short answer, then why it happens.
The short answer
Concrete shrinks a little as it cures, and where it is held in place it cracks. A control joint is a deliberate groove cut or tooled across the slab so that the crack happens there, in a straight line you hardly notice, instead of wandering across the surface. The joints go in soon after finishing, about a quarter of the slab's depth, and are spaced so that the panels between them stay roughly square. They reduce random cracking. They do not guarantee there will be none.
Why concrete cracks and why a joint helps
Concrete is mixed wet and gets stiff as it cures.
During that time it loses water and shrinks. A slab that is free to move can shrink without trouble, but a slab sitting on the ground, tied to a wall or locked at the corners is held back, and that restraint builds stress. When the stress exceeds what the concrete can bear, it cracks.
You cannot prevent the shrinkage, and it is hard to remove the restraint. What you can do is decide where the cracking happens. A control joint is a planned weak line. The concrete is thinner there, so the stress finds it first, and the crack forms under the joint and out of sight.
The result is a crack that is straight, tight and below the surface, instead of a diagonal one across the middle of the patio.
Step 2 of 3
See it
Each picture sits right after the section it explains.
See itIllustrates section 01: Why concrete cracks and why a joint helps
Watch it happen
Why a joint helps
A restrained slab cracks where it is stressed. A saw-cut joint is a planned weak line, so the crack forms under it, straight and out of sight.
1. Held back, it builds stress
A slab sitting on the ground, tied to a wall or locked at the corners is held back, and that restraint builds stress. When the stress exceeds what the concrete can bear, it cracks.
2. A planned weak line
A control joint is a planned weak line. The concrete is thinner there, so the stress finds it first.
3. Straight, tight, below the surface
The crack forms under the joint and out of sight. The result is a crack that is straight, tight and below the surface, instead of a diagonal one across the middle of the patio.
How deep and how soon
A joint has to be deep enough to work.
The usual rule of thumb is about a quarter of the slab's thickness. A joint that is too shallow does not draw the crack, and the concrete finds its own way instead.
Timing matters as much. Joints are tooled into the wet surface during finishing, or cut with a saw soon after the concrete has hardened enough to be cut without ravelling the edges. Wait too long and the concrete will already have cracked somewhere else.
That is why joint work is part of the schedule on the day of the pour, not an afterthought. A crew that is thinking about joints is planning the whole day around curing and weather.
See itIllustrates section 02: How deep and how soon
Watch it happen
How deep and how soon
A joint about a quarter of the slab's thickness draws the crack. A shallow joint does not, and a joint cut too late comes after the slab has already cracked.
1. About a quarter of the thickness
A joint has to be deep enough to work. The usual rule of thumb is about a quarter of the slab's thickness.
2. Too shallow, the crack goes elsewhere
A joint that is too shallow does not draw the crack, and the concrete finds its own way instead.
3. Cut soon after it hardens
Joints are tooled into the wet surface during finishing, or cut with a saw soon after the concrete has hardened enough to be cut without ravelling the edges.
How far apart and in what shape
Spacing depends on thickness. A common rule of thumb is roughly 2 to 3 feet of spacing for every inch of slab thickness, kept closer to 2 to 2.5 for better control.
On a 4 inch slab that is about 8 to 10 feet. Thinner slabs need joints closer together.
Shape matters too. The panels the joints create should be close to square. Long, narrow panels crack across their width more readily, so a joint layout that produces a ten foot by thirty foot strip invites a crack in the middle.
Layout is a judgment call that takes the whole slab into account, including its edges, the steps and how it will be used. A driveway that carries cars is laid out differently from a small stoop.
See itIllustrates section 03: How far apart and in what shape
Watch it happen
Spacing and shape
Joints that make panels close to square, and a layout with long narrow panels that crack across the middle.
1. Panels close to square
The panels the joints create should be close to square.
2. Long panels crack across
Long, narrow panels crack across their width more readily, so a joint layout that produces a ten foot by thirty foot strip invites a crack in the middle.
Corners, walls and the places that need extra care
Some spots are natural crack starters.
An inside corner, where the slab turns around an obstacle, concentrates stress, and a crack almost always starts from it. A joint is usually placed so that it runs to that corner, which gives the crack a line to follow.
Where the slab meets a house wall, a step, a post or a drain, a different kind of joint is used. An isolation joint, which has a compressible filler, lets the slab move independently from the structure. Control joints and isolation joints do different jobs, and mixing them up leads to trouble.
Look at the edges of a good patio and you can often see the pattern: joints that meet the corners, isolation strips along the house and straight, even panels in between.
See itIllustrates section 04: Corners, walls and the places that need extra care
Watch it happen
Control joints and isolation joints
Where a slab meets a house wall, a compressible filler lets it move on its own. The saw-cut joints do a different job.
1. Where the slab meets a wall
Where the slab meets a house wall, a step, a post or a drain, a different kind of joint is used.
2. An isolation joint
An isolation joint, which has a compressible filler, lets the slab move independently from the structure.
3. Two joints, two jobs
Control joints and isolation joints do different jobs, and mixing them up leads to trouble.
What joints do not do
A control joint reduces random cracking, but it does not make a slab crack free.
Poor base preparation, too much water in the mix, weak concrete or heavy loads can crack panels even with well placed joints. And sometimes a crack forms beside the joint rather than under it.
Joints can also fail on their own. They can fill with dirt and plants, and open edges can chip. Sealing them with a flexible sealant keeps water and debris out, and it is a maintenance item that needs renewing over time.
If your slab has cracked, the question is whether the crack is a hairline in a place where the joint should have been, or something larger tied to settlement. The first is cosmetic. The second needs a closer look.
See itIllustrates section 05: What joints do not do
Watch it happen
What joints do not do
A cracked panel beside a joint, and a flexible sealant run along each joint to keep water and debris out.
1. Fewer random cracks, not none
A control joint reduces random cracking, but it does not make a slab crack free.
2. Seal the joints
Sealing them with a flexible sealant keeps water and debris out, and it is a maintenance item that needs renewing over time.
What to ask when you plan a pour
Ask where the joints will go and why.
A good answer refers to the slab thickness, the shape of the panels and the corners. A poor answer is that they put them in wherever they fit.
Ask also how soon they are cut and how the concrete will be cured afterward. If you have an existing slab that has cracked, send photos with a note on where and when the cracks appeared, and we will say whether it looks like normal shrinkage or something more.
Step 3 of 3
Act on it
Quick answers, where to read next, and how we can help.
Questions people ask
What is a control joint in concrete?
It is a groove cut or tooled across the slab to create a weak line. When the concrete shrinks and cracks, the crack follows the groove instead of wandering across the surface.
How deep should a control joint be?
As a rule of thumb, about a quarter of the slab's thickness. A shallower joint may not guide the crack, and a very deep one can weaken the slab.
Does my slab still crack if it has joints?
It can. Joints reduce random cracking but do not eliminate it. Base problems, weak concrete or heavy loads can still crack a panel, sometimes beside the joint.
What is the difference between a control joint and an isolation joint?
A control joint guides shrinkage cracks within the slab. An isolation joint, filled with a compressible strip, separates the slab from a wall, step or post so they can move independently.
Do I need to seal the joints?
Sealing with a flexible sealant keeps water and debris out and protects the edges. It is a maintenance item and will need renewing over the years.
Seeing this at your place?
Send us a few photos through the contact page and the chat there, and we'll tell you what we think.
Request an estimateOur masonry and concrete workAll guides
Enduring On Construction, a New Jersey general contractor. NJ home improvement contractor registration 13VH13745900.