Step 1 of 3
Understand it
The short answer, then why it happens.
The short answer
Polymeric sand is fine sand mixed with a binder. Swept into the joints between pavers and lightly wetted, the binder activates and the sand hardens into a firm, flexible filler that resists weeds, ants and being washed away. It fails when the joints are not filled to the top, when the surface is soaked too hard or too soon, when it rains before it cures, or when water pours across the joints all year. It is a maintenance material and does not last forever.
What polymeric sand is and what it does
Ordinary joint sand is loose. It sits between the pavers and holds them in place against each other, but rain and runoff can carry it away, ants can tunnel through it and seeds can sprout in it. Polymeric sand adds a binder to the fine sand, so that when it is wetted, the particles stick together as it dries.
The cured joint is firmer than loose sand but is still slightly flexible, which matters because paving moves a little with temperature and load. A rigid filler would crack. A flexible one flexes.
The benefits are real: fewer weeds, less ant activity, less washing out of the joint and a surface that stays tight longer. They depend entirely on the product being installed well.
Our workHow it is installed
The joints have to be clean and dry, with the pavers dry too.
The sand is spread across the surface and swept into the joints until they are full to near the top, then the surface is compacted lightly so the sand settles, and more is swept in until the joints stay full.
The surface is then swept or blown clear, with special care at the paver faces. Any sand left on top will be wetted along with the rest, and the binder can leave a haze that is hard to remove. This is a common cause of the cloudy look on a new patio. Haze left to dry can be hard to remove, though some weathers off or can be cleaned off with a cleaner made for it.
Finally the sand is activated with water, using a fine mist that wets the joints without flooding them. The maker's instructions give the amount and the number of passes, and following them closely matters.
Why it washes out
The first cause is incomplete filling.
If the joints are not full to the top, the sand sits low, and the binder has less to grip. Rain then runs into the gap and carries the top layer away.
The second is too much water at the start. A heavy spray can wash the binder from the upper part of the joint, leaving loose sand behind. The third is rain too soon. The product needs a dry period after installation to cure, and rain in that window can ruin it.
The fourth is where the water goes. A patio that sheds water across the joints in a sheet, or a downspout that empties onto the paving, can wear out any joint filler. That points to a drainage problem, and sand alone will not fix it.
Step 2 of 3
See it
Each picture sits right after the section it explains.
See itIllustrates section 03: Why it washes out
Watch it happen
Why polymeric sand washes out
Joints that are not full, or water running across and under the paving, wear out the joint filler, and a moving base keeps opening the joints.
1. Joints full to near the top
The sand is swept into the joints until they are full to near the top.
2. A surface that is holding
A cured joint is firmer than loose sand but is still slightly flexible.
3. Water finds the joints
A patio that sheds water across the joints in a sheet will wear out any joint filler. That is a drainage problem, and no sand will fix it.
4. The base is moving
If the pavers themselves are sinking or uneven, the joints will keep opening and the sand will keep failing.
Joint size and paving condition
Polymeric sand works best in joints of moderate width.
Very wide joints do not hold it as well, and very narrow ones do not take enough sand to bind properly. If the pavers have shifted, or the joints have opened to different widths, the result will be uneven.
Depth matters too. The sand needs enough depth to grip. In shallow joints, such as those on thin or chipped pavers, it tends to lift out.
If the pavers themselves are sinking or uneven, the joints will keep opening and the sand will keep failing. That can point to a base problem, and more sand alone will not fix it.
Weather, timing and maintenance
Check the weather before starting.
The product needs dry conditions before and after installation, and a minimum temperature stated by the maker. A forecast with rain in the next day or two is a reason to wait.
Over time the sand wears. In sunny, well drained spots it can last for years, and in damp or shaded areas it may need attention sooner. When it does fail, the old sand can be cleaned out of the top of the joints and fresh product applied. It is routine upkeep and a lot less work than resetting a patio.
Weeds will still show up in some joints, since seeds can land on top of the cured sand. Pulling them early is easy. Letting them grow breaks up the joint.
How to tell if yours was done right
Look at the joints after the first season.
They should be full, firm and slightly below the paver edge. If they are low, crumbly or washed out in the places where water flows, the installation or the drainage needs attention.
A hazy film on the paver faces suggests that the surface was not swept clean before wetting. That can sometimes be treated, but the earlier the better.
If you are not sure what you have, send us photos of the joints and a note on how long ago the patio was laid and what the weather was. That is a good start for a first read on whether a refill will do or whether the problem lies deeper.
Step 3 of 3
Act on it
Quick answers, where to read next, and how we can help.
Questions people ask
What is polymeric sand made of?
Fine sand blended with a binder that activates with water. When wetted and dried, the particles bond into a firm but slightly flexible joint filler.
Why did my polymeric sand wash out after one rain?
Common reasons include joints that were not filled to the top, too much water at installation, or rain before it cured. Water pouring across the joints can also wear it away.
Why is there a white haze on my new pavers?
Sand left on the surface was wetted along with the joints, and the binder dried on the face. Sweeping or blowing the surface thoroughly before wetting prevents it.
Does polymeric sand stop weeds completely?
It reduces them a great deal, but seeds can still land and sprout on top of the cured sand. Pulling small weeds early keeps the joints intact.
Can I add polymeric sand over old sand?
Only if the old sand is cleaned out of the top of the joints first. The new product needs depth to grip and clean sides to bond to.
Seeing this at your place?
Send us a few photos through the contact page and the chat there, and we'll tell you what we think.
Request an estimateOur masonry and hardscape workAll guides
Enduring On Construction, a New Jersey general contractor. NJ home improvement contractor registration 13VH13745900.