Concrete Salt Damage: Why Scaling Happens and How to Slow It

That pitted, peeling top layer on a winter worn slab is scaling. What salt and freezing do to the surface, who is most at risk and how to slow it.

Step 1 of 3

Understand it

The short answer, then why it happens.

The short answer

Scaling is the flaking away of the top layer of a concrete slab, leaving a rough, pitted surface. It happens when water soaked into the surface freezes, and de-icing salt makes it worse by keeping that water in play through more freeze and thaw cycles. New slabs, weak surfaces and concrete without a proper air system are the most exposed. You slow it by avoiding salt on young concrete, sealing a sound surface and keeping water from standing on it.

What scaling looks like

A scaled slab has lost its smooth top skin.

At first the surface looks pitted or rough, as if it were sandblasted. In bad cases the cream is gone and the stone in the mix shows through. Flakes the size of a coin or larger may break off, particularly at edges and joints.

It is a surface problem and not usually a structural one, but it makes the slab look worn out, and it gets worse each winter as it opens more surface to water.

Step 2 of 3

See it

Each picture sits right after the section it explains.

See itIllustrates section 01: What scaling looks like

What scaling looks like

A slab with a smooth top skin that turns pitted and rough, then flakes break off at the surface and joints.

  1. 1. A smooth top skin

    A scaled slab has lost its smooth top skin.

  2. 2. Pitted and rough

    At first the surface looks pitted or rough, as if it were sandblasted. In bad cases the cream is gone and the stone in the mix shows through.

  3. 3. Flakes break off

    Flakes the size of a coin or larger may break off, particularly at edges and joints.

NextWhat causes it and who is at risk

What causes it and who is at risk

Concrete is porous. It absorbs water, and when that water freezes it expands and pushes on the surrounding concrete.

A strong, well made surface has tiny air pockets that give the ice room to expand. A weak surface does not, and the ice pops off the top layer.

Salt gets blamed, and it is involved, but mostly indirectly. Salty water holds moisture in the surface longer, draws water in, and sends the slab through more rounds of freezing and thawing. Each round is a chance for damage. Rock salt (sodium chloride) mostly harms concrete by multiplying freeze-thaw cycles and by corroding any steel in it. It does not chemically dissolve the concrete. Other chloride de-icers can be harsher.

Slabs poured late in the year, which have not had time to gain strength before the first salt. Slabs whose surface was weakened by too much water in the finish, by early drying or by being worked while bleed water was on top. Slabs with no air entrainment in the mix. And slabs where water stands, since standing water is the fuel.

That is why one driveway in a street scales and its neighbor does not. The salt was the same. The concrete was not.

See itIllustrates section 02: What causes it and who is at risk

How freezing water scales a slab

Salty water soaks into the porous surface, freezes and pushes on the concrete just under the skin, and the ice pops the top layer off. Salt keeps the cycle going.

  1. 1. Concrete is porous

    Concrete is porous. It absorbs water.

  2. 2. The water freezes

    When that water freezes it expands and pushes on the surrounding concrete.

  3. 3. The ice pops the top layer off

    A strong, well made surface has tiny air pockets that give the ice room to expand. A weak surface does not, and the ice pops off the top layer.

  4. 4. Salt keeps the cycle going

    Salty water holds moisture in the surface longer, draws water in, and sends the slab through more rounds of freezing and thawing. Each round is a chance for damage.

NextAir entrainment and why it matters

Air entrainment and why it matters

For outdoor concrete in a freezing climate, the mix should contain an admixture that creates a network of microscopic air bubbles.

They are too small to see, and they give freezing water room to expand without breaking the surface.

It is one of the cheapest protections there is, and it can only be added when the concrete is made. You cannot retrofit it. When you are having flatwork poured, it is a fair question whether the mix is air entrained.

See itIllustrates section 03: Air entrainment and why it matters

Why air entrainment matters

A network of microscopic air bubbles gives freezing water room to expand without breaking the surface.

  1. 1. A network of microscopic bubbles

    For outdoor concrete in a freezing climate, the mix should contain an admixture that creates a network of microscopic air bubbles. They are too small to see.

  2. 2. Room to expand

    They give freezing water room to expand without breaking the surface.

NextHow to slow it down

How to slow it down

Keep salt off new concrete through its first winter.

Use sand or a traction product instead and shovel early. On older sound concrete, use salt sparingly and sweep up the leftovers once the ice has gone, so it does not stay in the surface.

Be careful with some de-icers sold as concrete safe. Check what they contain, and avoid products reported to attack concrete.

Keep water moving off the slab. A surface that drains and does not hold puddles gets less water in the first place.

NextSealing, rinsing and spring care

Sealing, rinsing and spring care

A penetrating sealer applied to a sound, dry, clean surface slows the intake of water and salt.

It is not a cure, it wears, and it needs to be reapplied. It is also much less useful on a surface that has already scaled, since there is little left to protect.

Think of it as upkeep that buys time, best done before the damage starts.

NextWhat to do about a scaled slab

What to do about a scaled slab

Light scaling on a slab that is otherwise sound is sometimes treated with a thin resurfacing layer, though that depends on the slab underneath.

Heavy scaling with deep loss of surface, or a slab with other problems, may be a candidate for replacement. We cover how to decide in our guide to resurfacing and replacing.

Send us a photo of the slab and tell us how old it is and how it has been treated in winter. We will tell you what we see.

The salt left on a slab at the end of winter keeps working. As the weather warms and cools, it draws moisture into the surface and sets the damage in motion again. Sweep up any visible salt and sand in early spring, and rinse the surface with clean water if you can, taking care that the runoff goes somewhere that can drain.

Look at the slab once the ice has gone. Mark scaled patches, edges that have crumbled and joints that have opened, so you can compare next year. Early damage is easy to deal with. A year of neglect makes it a bigger job.

Keep an eye on the garage door and any trim that sits on or near the slab. Salt spray and splash will mark those too, and it is a good prompt to check the whole area.

See itIllustrates section 06: What to do about a scaled slab

A thin resurfacing layer for light scaling

A scaled slab with a thin cement-based layer troweled over it.

  1. 1. A scaled slab

    Light scaling can often be repaired with a thin resurfacing layer, if the slab beneath is sound.

  2. 2. A thin layer on top

    Light scaling can often be repaired with a thin resurfacing layer, if the slab beneath is sound. Heavy scaling with deep loss of surface, or a slab with other problems, may be a candidate for replacement.

NextQuestions people ask

Step 3 of 3

Act on it

Quick answers, where to read next, and how we can help.

Questions people ask

Is rock salt worse than other de-icers?

All of them add to freeze and thaw cycles. Some chemical de-icers are reported to damage concrete directly, so it is worth checking the product. The safest choice on new concrete is no de-icer at all.

Why did my new driveway scale in its first winter?

Often because it was poured late and had little time to gain strength, or because the surface was weakened when finished. Salt on a young slab is a common trigger.

Can scaling be stopped once it starts?

It can be slowed by sealing and by keeping salt and water off, but the lost surface does not come back. Repair generally means resurfacing or replacing.

Do pavers suffer from salt the same way?

Pavers are made differently, but salt can still affect the surface and the joints. Our guide to freeze and thaw covers the differences.

Is sand a good substitute for salt?

It gives traction but does not melt ice. For new concrete it is the safer choice. Sweep it up in spring so it does not clog drains.

Does the type of finish change how it handles salt?

A smooth, hard trowel finish is denser but can be slippery, while a broom finish gives grip. Neither is immune. What matters most is the mix and the way it was finished and cured.

Seeing this at your place?

Send us a few photos through the contact page and the chat there, and we'll tell you what we think.

Request an estimate

Our masonry and concrete workAll guides

Enduring On Construction, a New Jersey general contractor. NJ home improvement contractor registration 13VH13745900.

Send us the job

Drawings, or a building that needs work. We will come and look at it with you.

Enduring On Construction

Enduring On LLC, license, registration and contact details

Contractor

Enduring On Construction

Enduring On LLC · New Jersey general contractor

Home improvement

13VH13745900

NJ Div. of Consumer Affairs

Public works

753861

NJ Dept. of Labor

New home builder

0058509

NJ Dept. of Community Affairs

Based

Clark, New Jersey

Fully insured, with certificates and additional-insured endorsements issued on request. Registered with the New Jersey Department of Labor to perform public work at prevailing wage.

Verifiable with the State of New Jersey